Yesterday, I made a “scrunched” fabric cuff bracelet. The body of the cuff is made from fine silver and the frame is sterling.

Using fine silver allow the folds to happen without the work hardening and potential cracking to occur. The sterling silver frame adds some rigidity – you could use fine silver too but to prevent the cuff from bending out of shape too easily, so using sterling and its work hardening propensity, keeps the cuff in shape.

Read the rest over at The Adventurous Silversmith and see what happened with the LOS….