While I was at the dentist a couple weeks ago, the dental assistant asked me to make her a ring with a stone that she had in another ring. She brought in her current ring (cats eye cabochon) with the stone in a four prong setting that was made for a faceted stone. So I have crafted a bezel ring with 9 gauge Sterling Silver to form the shank. and here it is…….
Thanks for looking,
John
John Rasmussen
Lapidary, Artisan Jeweler at Rasmussen Gems and Jewelry LLC
66 year old retired educator (geology and emergency medical care) and practicing paramedic. I came back to my passion, rocks and minerals, then making gemstones and jewelry with them.