Here are some pictures of my most recent piece, which is actually serial #2, a duplication of serial #1, which was made in 2005. I couldn’t really remember how I made the first one, which turned out to be a good thing, because this one came out better. Having made 40+ pet urns in the last two years has really honed my skills. This piece is 11 inches long and made from 16 gauge brass sheet.