New York – The Gallery at Reinstein|Ross is pleased to present Amy West: RiverStones, an exciting exhibition of glass works from Murano, Italy. The exhibition will include vessels and jewelry from Amy West’s most recent body of work, entitled RiverStones. The work is inspired by the river Ardo, tributary to the Piave river in the Veneto. West describes the river as a source of peace, relaxation and inspiration. The light of the river, the movement of the current, the color of the rocks, and the beauty of the tumbled stones are all cited as inspiration. West says “The river is alive, and it makes its presence known to those paying attention.” While comforting however, the river’s constancy and strength is accompanied by dramatic change and shift. All of these expressions from the river are seen by West as metaphors for how we are tumbled and shaped by life, hopefully to come out of our personal experiences as rounded and smooth as the stones of the riverbed.
West says, “These pieces – vessels and jewelry – are reflections of the colors, the light, the shapes and forms that have filled my mind since before this collection started forming five years ago.”
West’s process begins with loose sketches, and then vessels are blown by hand of traditional Murano glass. For the RiverStones Collection, glass from the studio of Pino Signoretto was used. In some cases, once a vessel was blown and shaped, a kind of “Calcedonia” (multi-colored striation effect) is swirled around the vessel, to reflect the movement of the water, and dynamics of its flow. In other cases, the glass colors are actually combined during the glass gathering, and swirled in the blowing process.
After tempering, West begins the process of carving and cutting to texture and sculpt the glass. West specializes in Battuto (literally meaning “beaten” in Italian), the Murano style of cold-working glass, using diamond and stone wheels, to add detail, surface and texture that cannot be achieved in hot glass. This process can be very involved, and can extend to ten, twenty, or more stages of wheels, texturing and polishing.
The exhibition, RiverStones, is not only about vessels, but has a distinct focus on jewelry. West’s jewelry for RiverStones, is derived from the same materials, processes and inspiration, but is created to be personal.
The exhibition, Amy West:RiverStones, will also include large projections of her work, sketches, photographs of Murano, and the Ardo River, the inspiration for this exciting body of work.
Born and raised in the Midwest, Amy West has studied, worked and lived on four continents. Her work draws on her vast experiences in cultures from around the world, and expresses a vision that is truly her own.
Prior to arriving in New York for this exhibition, some of West’s current work was on display at the Palazzo da Mula, in an exhibit – Gruppo 30141 Murano – recognizing Glass Masters of Murano. In the summer of 2015, she will be artist in residence at the Corning Museum of Glass in Corning, New York. The Gallery at Reinstein|Ross is proud to present Amy West’s work in New York City. This is her first solo exhibition.
The Gallery at Reinstein|Ross
30 Gansevoort Street
New York, NY 10014
212.226.4513
ReinsteinRoss.com
Robyn Hawk
Latest posts by Robyn Hawk (see all)
- BrilliAnt®, the 8th edition of the ADTF, Goes International - August 13, 2016
- AGTA Spectrum Awards™ "Platinum Honors" Winnners #AGTA15 - August 11, 2016
- YES! an #Olympic #Jewelry Story! It Happened In The Pool #JewelryMoment - August 9, 2016