﻿{"id":14,"date":"2007-11-15T23:04:00","date_gmt":"2007-11-16T04:04:00","guid":{"rendered":"http:\/\/freeforged.userblogs.ganoksin.coms\/2007\/11\/15\/casting\/"},"modified":"2007-11-15T23:04:00","modified_gmt":"2007-11-16T04:04:00","slug":"casting","status":"publish","type":"post","link":"https:\/\/userblogs.ganoksin.com\/freeforged\/2007\/11\/15\/casting\/","title":{"rendered":"Casting"},"content":{"rendered":"<p><span style=\"font-family: georgia\">So it&#8217;s been awhile since my last post, oops. To be fair, I have been a bit busy learning a new technique &#8211; Cuttlebone Casting. I did not have any real previous experience with casting before, but for my current project I wanted to have an element that was cast with the cuttlefish bone method. Casting with a cuttlefish bone imparts a unique texture on the piece, something that cannot be obtained any other way, and is a method that has been used for casting by gold- and silversmiths for many many years. It took me five tries to get one that was complete, but eventually I did it! Sorry, no pictures yet, but I hope to have the piece finished by next week and will post some pictures then. <\/span><br \/><span style=\"font-family: georgia\">Until then, check out this example of a <\/span><a href=\"http:\/\/www.etsy.com\/view_listing.php?listing_id=7258205\">cuttlefish casting<\/a><span style=\"font-family: georgia\"> in <\/span><a href=\"http:\/\/www.etsy.com\/shop.php?user_id=100235\">Mooretaste&#8217;s shop<\/a><span style=\"font-family: georgia\">. <\/span><\/p>\n","protected":false},"excerpt":{"rendered":"<p>So it&#8217;s been awhile since my last post, oops. To be fair, I have been a bit busy learning a new technique &#8211; Cuttlebone Casting. I did not have any real previous experience with casting before, but for my current project I wanted to have an element that was cast with the cuttlefish bone method. [&hellip;]<\/p>\n","protected":false},"author":85,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[1],"tags":[],"_links":{"self":[{"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/posts\/14"}],"collection":[{"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/users\/85"}],"replies":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/comments?post=14"}],"version-history":[{"count":0,"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/posts\/14\/revisions"}],"wp:attachment":[{"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/media?parent=14"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/categories?post=14"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/freeforged\/wp-json\/wp\/v2\/tags?post=14"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}