I’ve made two 18ga, etched, sterling cuff bracelets for a client. I’m able to draw out the desired names & symbols, adher it to heavy sterling, acid etch for 10 hrs., shape in the hydraulic press, and patina. I also engraved chosen verses on the back. Perfect one of a kind gifts.