﻿{"id":11,"date":"2009-11-18T23:25:14","date_gmt":"2009-11-19T04:25:14","guid":{"rendered":"http:\/\/jaywhaley.userblogs.ganoksin.coms\/?p=11"},"modified":"2009-11-18T23:25:14","modified_gmt":"2009-11-19T04:25:14","slug":"metalclay-fistfight","status":"publish","type":"post","link":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/2009\/11\/18\/metalclay-fistfight\/","title":{"rendered":"metalclay fistfight&#8230;"},"content":{"rendered":"<p>Oh I am about to get in the middle of a fight!\u00a0<\/p>\n<p>While I have not worked with metalclay, I know a fair amount about it.\u00a0 However, I am learning a lot more about it recently.<\/p>\n<p>Kate McKinnon, who I will interview tomorrow on my BlogTalkRadio Show,\u00a0 is about to get a lot of metal clay people mad at her ( and me?).\u00a0 She claims precious metal clay needs to be adequately kiln fired, work hardened, etc., to be a real jewelry metal.\u00a0 She says the metal clay industry is deliberately mis-informing the metal clay community as to the proper techniques required.<\/p>\n<p>There are a lot of things going on in the metal clay world I didn&#8217;t know, but I&#8217;m going to find out tomorrow&#8230;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>Oh I am about to get in the middle of a fight!\u00a0 While I have not worked with metalclay, I know a fair amount about it.\u00a0 However, I am learning a lot more about it recently. Kate McKinnon, who I will interview tomorrow on my BlogTalkRadio Show,\u00a0 is about to get a lot of metal [&hellip;]<\/p>\n","protected":false},"author":138,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[1],"tags":[],"_links":{"self":[{"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/posts\/11"}],"collection":[{"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/users\/138"}],"replies":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/comments?post=11"}],"version-history":[{"count":2,"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/posts\/11\/revisions"}],"predecessor-version":[{"id":16,"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/posts\/11\/revisions\/16"}],"wp:attachment":[{"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/media?parent=11"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/categories?post=11"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/jaywhaley\/wp-json\/wp\/v2\/tags?post=11"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}