﻿{"id":56,"date":"2008-06-23T14:34:00","date_gmt":"2008-06-24T02:34:00","guid":{"rendered":"http:\/\/katherinemiess.userblogs.ganoksin.coms\/2008\/06\/23\/etruscan-chain-a-kick-in-the-pants-2\/"},"modified":"2008-06-23T14:34:00","modified_gmt":"2008-06-24T02:34:00","slug":"etruscan-chain-a-kick-in-the-pants-2","status":"publish","type":"post","link":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/2008\/06\/23\/etruscan-chain-a-kick-in-the-pants-2\/","title":{"rendered":"Etruscan Chain- A Kick in the Pants"},"content":{"rendered":"<p><a href=\"http:\/\/bp3.blogger.com\/_2h_6OEZccWc\/SFsYPuOAS0I\/AAAAAAAAAKo\/nx3nOQ65RaA\/s1600-h\/june+19+2008+jewelry+025.JPG\"><img loading=\"lazy\" height=\"236\" alt=\"\" src=\"http:\/\/bp3.blogger.com\/_2h_6OEZccWc\/SFsYPuOAS0I\/AAAAAAAAAKo\/nx3nOQ65RaA\/s400\/june+19+2008+jewelry+025.JPG\" width=\"471\" border=\"0\" \/><\/a><\/p>\n<p>My Etruscan chain&#8230; So beautiful, so time consuming. After two years of looking at this chain, I don&#8217;t know what to do with it. Maybe a little post about this tedious, and intimidating project will help me to finish it. <\/p>\n<div><a href=\"http:\/\/bp2.blogger.com\/_2h_6OEZccWc\/SGBhV0FFa8I\/AAAAAAAAALg\/ydhpOHt_xxI\/s1600-h\/chain+links.jpg\"><img alt=\"\" src=\"http:\/\/bp2.blogger.com\/_2h_6OEZccWc\/SGBhV0FFa8I\/AAAAAAAAALg\/ydhpOHt_xxI\/s200\/chain+links.jpg\" border=\"0\" \/><\/a><a href=\"http:\/\/bp2.blogger.com\/_2h_6OEZccWc\/SGBc1z9hlQI\/AAAAAAAAALQ\/kkCIh-90uNw\/s1600-h\/chain+links.jpg\"><\/a><\/div>\n<div>This 7 .5&#8243; fine silver bracelet took about 3 dedicated months to weave between my full time job, and school. Each jump ring was shaped, and fused by hand. Hundreds of rings- a good number melted. Hundreds of links-many which snapped, and hours of weaving, loop, after loop, after work-hardened loop. It is a masterpiece, an ancient technique replicated by my own two prematurely arthritic hands.<\/div>\n<div><\/div>\n<div>Now, just what the heck do I do with it?! <\/div>\n<div><a href=\"http:\/\/bp2.blogger.com\/_2h_6OEZccWc\/SGBc1z9hlQI\/AAAAAAAAALQ\/kkCIh-90uNw\/s1600-h\/chain+links.jpg\"><\/a><\/div>\n<div><\/div>\n","protected":false},"excerpt":{"rendered":"<p>My Etruscan chain&#8230; So beautiful, so time consuming. After two years of looking at this chain, I don&#8217;t know what to do with it. Maybe a little post about this tedious, and intimidating project will help me to finish it. This 7 .5&#8243; fine silver bracelet took about 3 dedicated months to weave between my [&hellip;]<\/p>\n","protected":false},"author":68,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[1],"tags":[],"_links":{"self":[{"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/posts\/56"}],"collection":[{"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/users\/68"}],"replies":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/comments?post=56"}],"version-history":[{"count":0,"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/posts\/56\/revisions"}],"wp:attachment":[{"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/media?parent=56"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/categories?post=56"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/katherinemiess\/wp-json\/wp\/v2\/tags?post=56"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}