It’s a little known fact that you can clean your silver jewelry perfectly with a simple solution called Tarnex available at most hardware/home improvement stores. Tarnex smells bad and is too harsh of a chemical to be used around pearls, amber and other soft organic jewelry materials. However it does not effect harder gemstones like topaz, garnet, etc…,
Simply pour a little tarnex in a glass container, dip the silver jewelry in and rinse with water. the tarnish should be removed instantly. For a deep clean, brush with toothbrush and soapy water after Tarnex.