{"id":320,"date":"2017-03-28T10:14:51","date_gmt":"2017-03-28T15:14:51","guid":{"rendered":"http:\/\/userblogs.ganoksin.com\/lillianjones\/?p=320"},"modified":"2017-03-29T08:35:26","modified_gmt":"2017-03-29T13:35:26","slug":"basse-taille-cloisonne-pendant-part-iv","status":"publish","type":"post","link":"https:\/\/userblogs.ganoksin.com\/lillianjones\/2017\/03\/28\/basse-taille-cloisonne-pendant-part-iv\/","title":{"rendered":"Basse Taille and Cloisonne Pendant: Part IV"},"content":{"rendered":"<table style=\"height: 3626px;width: 531px\">\n<tbody>\n<tr>\n<td style=\"width: 521px\">I am now adding the first layers of enamel.\u00a0 Although I will not photograph all the layers, it will take may 10 layers or so to fill it.\u00a0 You could pile it in, but it is better to layer thinly, and you can change the colors as you work your image.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele1.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-331\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele1.jpg\" alt=\"Triskele1\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele1.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele1-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/p>\n<p>Enamel on most any metal requires that you put a coat of glass on the back of the metal, to balance out the coefficent of expansion differences between the metal and the glass.\u00a0 Most enamels that you purchase have an expansion rate designed to work with silver or copper, and if you are doing stained glass (enamel on glass) that is a different expansion, and different enamels.\u00a0 Here I am applying black enamel to the back.\u00a0 In short, if I don&#8217;t, the front will crack and flake right off.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele2.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-332\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele2.jpg\" alt=\"Triskele2\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele2.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele2-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/p>\n<p>Here is the enamel, drying on top of my teeny tiny tabletop kiln.\u00a0 Since I make little things, I like this style of kiln.\u00a0 I can just put things in and out with tweezers, no walking around the room with a firing fork.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele3.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-333\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele3.jpg\" alt=\"Triskele3\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele3.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele3-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele4.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-334\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele4.jpg\" alt=\"Triskele4\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele4.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele4-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/p>\n<p>Here I am trying to capture the loose blue line in the original tattoo image, by adding enamel without the boundaries of the silver wire.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele5.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-335\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele5.jpg\" alt=\"Triskele5\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele5.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele5-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/p>\n<p>This is a cutout made by a punch that I used to create some silver detail for the back of the piece, just to make it a little more interesting.\u00a0 In case it turns over on the lady&#8217;s neck, there will still be something to look at.<br \/>\n<a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele6.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-336\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele6.jpg\" alt=\"Triskele6\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele6.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele6-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><br \/>\n<a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele7.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-337\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele7.jpg\" alt=\"Triskele7\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele7.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele7-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/p>\n<p>And here is the final project.\u00a0 I choose yellow to match her hair.<br \/>\n<a href=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele8.jpg\"><img loading=\"lazy\" class=\"alignleft size-full wp-image-338\" src=\"http:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele8.jpg\" alt=\"Triskele8\" width=\"576\" height=\"432\" srcset=\"https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele8.jpg 576w, https:\/\/userblogs.ganoksin.com\/lillianjones\/files\/2017\/03\/Triskele8-300x225.jpg 300w\" sizes=\"(max-width: 576px) 100vw, 576px\" \/><\/a><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>&nbsp;<\/p>\n","protected":false},"excerpt":{"rendered":"<p>I am now adding the first layers of enamel.\u00a0 Although I will not photograph all the layers, it will take may 10 layers or so to fill it.\u00a0 You could pile it in, but it is better to layer thinly, and you can change the colors as you work your image. Enamel on most any [&hellip;]<\/p>\n","protected":false},"author":174,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[1],"tags":[],"_links":{"self":[{"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/posts\/320"}],"collection":[{"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/users\/174"}],"replies":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/comments?post=320"}],"version-history":[{"count":14,"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/posts\/320\/revisions"}],"predecessor-version":[{"id":390,"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/posts\/320\/revisions\/390"}],"wp:attachment":[{"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/media?parent=320"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/categories?post=320"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/lillianjones\/wp-json\/wp\/v2\/tags?post=320"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}