﻿{"id":29,"date":"2010-05-09T18:42:32","date_gmt":"2010-05-09T23:42:32","guid":{"rendered":"http:\/\/mmaxwell.userblogs.ganoksin.coms\/?p=29"},"modified":"2010-05-09T18:42:32","modified_gmt":"2010-05-09T23:42:32","slug":"milling-bands","status":"publish","type":"post","link":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/2010\/05\/09\/milling-bands\/","title":{"rendered":"Milling bands"},"content":{"rendered":"<p>Bands are really easy with the JWX-30 mill.\u00a0 the models are milled on the rotary fixture as shown here.\u00a0 The wax is attached by sliding it on to the shaft of the fixture, and stays in place by means of friction.\u00a0 The screw fixture to the left of the shaft is used to remove the wax after milling, by rotating towards the wax and pushing it off without stressing the wax.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-fixture-01.jpg\"><img loading=\"lazy\" class=\"alignnone size-medium wp-image-30\" src=\"http:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-fixture-01-300x199.jpg\" alt=\"\" width=\"300\" height=\"199\" srcset=\"https:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-fixture-01-300x199.jpg 300w, https:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-fixture-01.jpg 500w\" sizes=\"(max-width: 300px) 100vw, 300px\" \/><\/a><\/p>\n<p>Many rings can be milled at once on this fixture.\u00a0 I milled both of these bands at the same time in a few hours.\u00a0 The inside of the bands will have to be hand finished to the proper finger size, but that is all the additional work needed before casting.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-rings-pair.jpg\"><img loading=\"lazy\" class=\"alignnone size-medium wp-image-31\" src=\"http:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-rings-pair-300x199.jpg\" alt=\"\" width=\"300\" height=\"199\" srcset=\"https:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-rings-pair-300x199.jpg 300w, https:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2010\/05\/rotary-rings-pair.jpg 500w\" sizes=\"(max-width: 300px) 100vw, 300px\" \/><\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>Bands are really easy with the JWX-30 mill.\u00a0 the models are milled on the rotary fixture as shown here.\u00a0 The wax is attached by sliding it on to the shaft of the fixture, and stays in place by means of friction.\u00a0 The screw fixture to the left of the shaft is used to remove the [&hellip;]<\/p>\n","protected":false},"author":146,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[1],"tags":[],"_links":{"self":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts\/29"}],"collection":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/users\/146"}],"replies":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/comments?post=29"}],"version-history":[{"count":1,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts\/29\/revisions"}],"predecessor-version":[{"id":32,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts\/29\/revisions\/32"}],"wp:attachment":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/media?parent=29"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/categories?post=29"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/tags?post=29"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}