﻿{"id":61,"date":"2011-03-02T23:14:24","date_gmt":"2011-03-03T04:14:24","guid":{"rendered":"http:\/\/mmaxwell.userblogs.ganoksin.coms\/?p=56"},"modified":"2011-03-02T23:14:24","modified_gmt":"2011-03-03T04:14:24","slug":"new-experiments-with-milling-wooden-jewelry","status":"publish","type":"post","link":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/2011\/03\/02\/new-experiments-with-milling-wooden-jewelry\/","title":{"rendered":"New experiments with milling wooden jewelry"},"content":{"rendered":"<p>I have been looking into the capacity for milling directly into exotic woods for finished jewelry items.\u00a0 I have milled rings already, as can be seen in the current March issue of MJSA magazine where I have a step by step article in &#8220;At the Bench&#8221; section.<\/p>\n<p>I Took a look at the construction of a bracelet my wife likes made from fused glass.\u00a0 I took the construction of the multi-segmented bracelet and designed a wooden one in CAD with a leaf and vine pattern that runs through all of the links.<\/p>\n<p>I began the milling here in cocoblo wood, but realized that the tighter grain of ebony was going to be a better material to show the subtle pattern.<\/p>\n<p>I placed three of the 12 bar shaped segments on one milling tool path.\u00a0 Here the roughing pass on the front is shown.<\/p>\n<p><a href=\"http:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2011\/03\/bracelet-milling-01.jpg\"><img loading=\"lazy\" class=\"alignnone size-medium wp-image-57\" src=\"http:\/\/userblogs.ganoksin.com\/mmaxwell\/files\/2011\/03\/bracelet-milling-01-300x199.jpg\" alt=\"\" width=\"300\" height=\"199\" \/><\/a><\/p>\n","protected":false},"excerpt":{"rendered":"<p>I have been looking into the capacity for milling directly into exotic woods for finished jewelry items.\u00a0 I have milled rings already, as can be seen in the current March issue of MJSA magazine where I have a step by step article in &#8220;At the Bench&#8221; section. I Took a look at the construction of [&hellip;]<\/p>\n","protected":false},"author":146,"featured_media":0,"comment_status":"open","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[1],"tags":[],"_links":{"self":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts\/61"}],"collection":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/users\/146"}],"replies":[{"embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/comments?post=61"}],"version-history":[{"count":1,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts\/61\/revisions"}],"predecessor-version":[{"id":59,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/posts\/61\/revisions\/59"}],"wp:attachment":[{"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/media?parent=61"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/categories?post=61"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/userblogs.ganoksin.com\/mmaxwell\/wp-json\/wp\/v2\/tags?post=61"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}