The Numbers

417 10K Gold

585 14 K Gold

750 18 K Gold

800 Silver

925 Sterling Silver

950/900 PLT

 

A good way to the “fine-ness”/percentage gold of any of these metals divide by pure metal (.024K)

Example: 14K Gold% .024 K= Roughly .585

Example: 10K/.024=750

 

Weight conversions

1 Pennyweight(DTW)=1.55 Grams

.643 Pennyweight(DTW)=1 gram Penny weight is a little more than a gram plus half itself

1Gram= .643 Pennyweight (DTW)

20 Pennyweights= 1 Troy ounce

31.1 grams= 1 Troy ounce

A good way to remember the conversion…. If someone can help me out, that would be fantastic!

 

 