I thought it would be fun to share this video of a bronze pouring (casting) done at Mission College (Santa Clara, CA) this spring. I’m the one on the right in the blue hard hat.
Enjoy!
[youtube]http://www.youtube.com/watch?v=d5C9ykfmO78[/youtube]
Below is a picture of my bronze casting just after being taken from the sand mold, with the gating still intact. It is a series of bronze bas relief mini-art pieces. I am still working on these pieces, but I will definitely post photos when I finish them.
Bronze casting