Basse Taille and Cloisonne Pendant:Part2

Continuing from the last post, I am now going to use the etched plate to create and fine silver base for the enamel. I could use a rolling mill, but that would distort the image. So I will use the hydraulic press instead, which applies pressure directly down and will not stretch the silver. I’ve […]