At the weekend I decided I had better get on and try the bronze clay. I have had a sample since last autumn but only recently bought the firing pan and charcoal. I have to say thanks to The Little Bead Shop as when I ordered charcoal from them it arrived in a stunning black and white spotty wrapping paper and my receipt had a pretty heart shaped bead tied to it with pink ribbon, it felt like a present! I had been warned that I may not like working with the bronze clay. Some of my friends know that I don’t really like to get dirty……. and I can’t say that I was very keen. My first attempt was to roll out a long sausage and wind it to make a bangle. Needless to say I could immediately see that fine cracks were appearing in the surface of the clay but carried on. I think perhaps it was a bit over-ambitious to start with this kind of thing but I wanted to do something that I could do with art clay silver. I also made a big chunky ‘c’ clasp and a few beads. The firing schedule is quite lengthy and when I opened the kiln I was not exactly thrilled by all the flakes of oxid
e dropping off the outside of the firing pan. I say it is being an enameller that makes me obsessively clean around my kiln – this may just be me making an excuse for myself of course. I wasn’t initially very keen on the colour of the finished pieces either, but polished off some of the patina and like them better now. I had been thinking I would use the clasp to make a beaded necklace, perhaps with the coral and transparent beads I made a few weeks ago. Unfortunately they don’t really go together…… typical! I am now going to have to make a set in greens or maybe topaz?
lynneglazzard
Latest posts by lynneglazzard (see all)
- More rings - January 27, 2010
- Ugthorpe hoard - January 27, 2010
- Does it have to be precious? - January 22, 2010
{ 1 comment… read it below or add one }
like my mums crazy packaging? lol xx