Once the pieces are all thoroughly dry I take a section of the dry tube and dip it quickly into clean water. I rub it firmly on the edge of the dry piece where I want to attach it and then hold it for a few seconds to allow it to connect firmly. I then return it to the hotplate to dry thoroughly and repeat the process with the remaining pieces.