To create a slight curve in the art clay silver pieces I place the freshly cut slabs of art clay silver over a ceramic mug to dry. This creates a very gentle curve of the right amount for a section of a bracelet.
Here the left hand piece is left smooth and the right hand section has been textured around the edge using a metal ball tool.