In the top and the left hand side pieces I have added fine silver wire and tiny round silver balls of fine silver to the surface of the fired art clay silver using silver overlay paste in order to create cells into which I can later add enamel.
The lower right hand piece has been water etched to create the cells.
After drying thoroughly these will be re-fired in the kiln at 800 degrees centigrade