I am currently in the middle of running an Art Clay Silver Level 1 Certification course which is, of course, taking up most of my time. I have had a chance to set up and fire a piece of glass in May’s big kiln though and here is the result. Although not a very inspired piece from a design point of view it has enabled me to check the firing temperature of the kiln and try out the new controller. I am not quite sure what to do with it now though…….
lynneglazzard
Latest posts by lynneglazzard (see all)
- More rings - January 27, 2010
- Ugthorpe hoard - January 27, 2010
- Does it have to be precious? - January 22, 2010
{ 3 comments… read them below or add one }
Ok so you will need to do a few more before you can reglaze the house 🙂
This piece is approx 250 x 240 mm
On pretty, how big is it? Can you slump it into a bowl or somethinmg maybe? Otherwise you will have to start replacing the house windows!!!