This post was supposed to be up 2 weeks ago but I’ve been lagging it. I don’t buy into the whole notion of saying ‘I don’t have time’, because you can always make time for anything you put your mind to. I either fire my secretary, which I don’t have, or I learn how to schedule myself better. Anyway, I always love coming up with different cuts that’s not in the norm. They’re usually special cuts to inspire that designer in us all. Shapes that you won’t find in the market because there isn’t a demand for that shape. Well, I was inspired to come up with this new cut that looks like a shield so I named it a shield cut because me being the artist/designer, I have to exercise my artistic freedom. If you have a vision I can shape your creation so feel free to ask me or send me your requests. Ok, enough selling myself, time for the good stuff.
First off, I’m a fan of Amethyst. One, it provides me with a wide range of that purple hue color that I’m a fan of. Two, It’s affordable and I have a that freedom of trial and error without killing my pockets. You can waste a lot of money if you’re not trained when mapping out where and how to cut your piece of rough so take your time and map out the steps when dealing with the cutting process.
So here’s my piece of rough I chose. This particular Amethyst is a ‘rose de france’ amethyst. The color is reminiscent of a lavender lilac shade which is a lighter color that usually comes from the Amethyst family.
This is the process of slicing. I need to slice this piece of rough in order to get my desired section I choose to preform the stone out of.
This diamond grade disk is spinning at a high RPM. Water is needed to cool off the friction this process causes.
Take your time when pushing the piece of rough through the disk. You don’t want to break the stone and don’t want to lose a finger in the process so be cautious if you ever decide to slice.
So I sliced through the rough and notice how clean it came out.
I displayed the two pieces of sliced Amethysts for an up-close, personal view so you can to check out the aftermath of the slicing process.
After the slicing process, I started to preform the Amethyst. I started the process by hand until I got the desired shape I’ve been looking for. I then transferred the stone to my dop stick (check out one of my older blogs by clicking on the link to get the terminology, I.E. ‘doping stick’ by clicking here.) for a more controlled and measured feel to the shape I was aiming for.
If you can see here, I’m cutting rounded inward grooves into the girdle (the side of the stone which separates the top from the bottom of the stone).
I got the rounded areas done. This is that time in this process where you really start to get excited by the way it’s starting to take shape.
The next step for this rose de france amethyst is to start cutting some facets into it.
I’m touching up the rounded sections on the girdle.
I added a regular table to the top of the amethyst but I wasn’t too pleased with the outcome so I decided to go with a double-sided checkerboard rosecut to the stone.
I love the ‘trial and error’ process. I’m honestly satisfied with the final product.
Why put the inward, rounded grooves into the stone you ask? I don’t know, maybe I can build something with bezels that snuggle perfectly into those grooves or have some sort of prong or build some weird bezel? Who knows, it all comes down to your artistic innovation – when that designer in you comes out to play.
Till next time…
sako
Latest posts by sako (see all)
- Fresh Water Elephant - March 5, 2014
- Spessartite Delight - August 15, 2013
- Orange shaped Triangle - January 3, 2013





















{ 2 comments… read them below or add one }
I love what you did to the stone, thank you for sharing.
Great pics, but they sort of jump from the detailed description on rough cutting to the finished facets. What did you cut the facets on? Was it freehand or did you use a facetor with a cheater?