Today was spent designing and cutting waxes as normal. This nice coin holder for a $2.5 dollar Gold Piece was easy but will make a real statement for the owner when finished.
In 18K Yellow Gold with 17 3mm Green Tourmaline around the coin, this should be an eye catcher. It will take about an hour to machine out the wax front and back. This one will be exciting to pull off the mill and clean up.
Just a note for those others out there working in Cad/Cam… SAVE YOUR WORK! I was almost finished with this when we had a power burp and lost everything. That cost about an hour!!!
Thats all for today. Thanks for blogging along with us!