The Anglo Saxon disk: Granulation on Silver

I’ve returned to the bench after a hiatus, and need to sharpen my skills in granulation.  As I love English history, and all things Game of Thrones, I will make a simplified Anglo Saxon Disk pendant. I start with a fine silver disk, size 1 and 1/8 inch, or about 29 mm.  The thickness of my […]

Torch Enameling: Cloisonne on Silver Part II

This is the last part of a tutorial on torch enameled cloisonne. In this picture I have picked a color pallet of green and blue and yellow.     And here I’ve filled the cells.   Firing with mapp gas, and a cheap little torch tip from Lowes.   And there it is, filled with […]

Simplifying Granulation

Lately I’ve been absorbed in making lots of earrings for the holiday season, using my new granulation skills. I’ve found fusing to be an easy and surprisingly speedy way to assemble things. Anyone who has experimented with granulation knows that the main problem is making the granules. My friend Iris solved this problem for me, […]

The Beauty of Portability: Working at the Beach

My friend Iris was in town this week, to enjoy the hurricane in Wilmington, NC. After it blew over, I joined her down at the Carolina coast for a few days of jewelry talk, fancy food and beach. Because this is our passion, we are both happiest while working. So she used her new technology […]

Enameling Again

Christmas is coming, and the elves are all doing production work, with the hope that someone, somewhere will have some money to spend. For the last week I’ve been making granulated earrings that all look alike. Not very entertaining…so this week I worked on a pair of enamel earrings for a sample for a class […]

Granulation meets Biology

Design is the final frontier of any technique. Making a personal statement with granulation is difficult, because granulation has definite character. This week’s earrings for the Betty McKim Earring Challenge uses multiple techniques, and begins to explore the nexus between geometry and biology. On my bench I have these bases to start with. Being a […]

From Geometry to Jellyfish

The past few years I have struggled with my affinity for the circle. It just seemed too easy, but recently I have decided to just go with it. After all, there are lots of interesting things that are circular: planets, hubcaps and hurricanes. This is one of a series of triskele enamels, with tri-fold symmetry. […]

Turning a Sow’s Ear into a Silk Purse

Gone are the days when I tossed my mistakes into the little box on my bench. Silver is just too expensive to treat without the proper respect, and perhaps that is as it should be. Even though anything that could go wrong did, I decided to fix the meltdown to use for my Betty McKim […]