Simplifying Granulation

Lately I’ve been absorbed in making lots of earrings for the holiday season, using my new granulation skills. I’ve found fusing to be an easy and surprisingly speedy way to assemble things. Anyone who has experimented with granulation knows that the main problem is making the granules. My friend Iris solved this problem for me, […]

Granulation using Plating

When fusing things together, I have realized that there are several approaches, that have their place. There is straight-up fusing, using just the torch. This is the best when you are trying to flow the metal across a gap. It requires a lot of heat control, because you are working mainly at melting temperature, and […]