bezel forming jigs for 22 ga., 1/4″ tall copper bezels . the bezels are intended to fit on top of parts cut from existing blanking dies . I made a separate die to cut parts slightly smaller than the existing parts, and soldered a stck of them together , about 3/8″ tall . these are screwed to the 1/2″ thick aluminum base plate . 3/32″ dia. holes are strategically placed in the base plate, to accept steel pins that aid in forming the bezel by keeping it where you put it, in certain places , basically.
sheltech
Latest posts by sheltech (see all)
- A Brief History of the RT/Pancake Die Universe - March 10, 2018
- The Timber Bay Embossed Butterfly - April 4, 2015
- Amazonite and Silver Set - August 8, 2014