Today is the first warm day in my studio since we’ve moved here. So what do I do, well, turn on the kiln of course!
I finally remembered to dome my fine silver blanks for the earrings I’ve had planned. I kept bringing them to work to dome with tools borrowed from zee boss, and then forgetting to do them! d’oh!
Now there are three earrings sets started. Yay!
I’m working on some creatures of the sea in the hopes of getting them in to some coast galleries and just ’cause I likes sea critters. It also doesn’t hurt that I have some wicked awesome blues in my enamel palette.
Adam’s peanut butter is essential to the enameling process, BTW.
This is how far I got today before my back started getting cranky:P

The Garibaldi fish makes me giggle.
~m